Selecting the right brazing alloy depends on more than base metal alone. Joint design, working temperature, performance requirements, certification needs, available forms and cost all influence the correct specification. Answer three questions below to get a specific recommendation, or read the guidance sections to understand the principles behind alloy selection.

How to Use This Guide

The selector asks three questions. First, which metals are you joining — this determines which alloy families are suitable and whether specialist flux is required. Second, what is your primary concern — this balances performance, cost, colour match or aerospace certification requirements. Third, how are you applying the alloy — rod, flux-coated rod, preforms or paste — which determines the form notes and any process-specific guidance.

The result shows the recommended alloy with silver content and melting range, the correct flux with its active range and EN standard, an application note for your chosen form, and an alternative where one exists. For stainless steel, nickel alloy and other specialist combinations, a warning note flags any critical requirements that must not be overlooked.

Find your alloy

Answer three questions to get a recommended alloy and flux combination for your application.

Base Metals

Base metals are the primary driver of alloy selection. The alloy must bond metallurgically to both base metals, and the flux must be capable of removing the oxide layers present on both surfaces at brazing temperature. Most standard combinations — copper, brass, bronze, mild steel — are served by general-purpose silver brazing alloys with GS30 flux. Stainless steel, nickel alloys and tungsten carbide require L-AG45SnSi or AG206 with Stay-Silv Black flux. Aluminium requires a completely different alloy family. Copper-to-copper joints can be served by self-fluxing copper phosphorus alloys, eliminating the need for separate flux entirely.

Silver Content

Silver content is the primary variable within the silver brazing alloy range. Higher silver content lowers the melting point, improves fluidity and increases joint ductility — at higher material cost. AG103 at 55% silver is the most versatile and highest-performing general-purpose grade. AG107 at 30% silver is a widely used mid-range grade balancing performance and cost. AG205 through AG207 are economy grades for high-volume, less-critical applications. The selector accounts for your priority — whether you are optimising for performance, seeking a cost-balanced specification, or minimising material cost.

Certification Requirements

For aerospace applications, materials must be supplied with full certification and batch traceability documentation, and not every standard EN1044 grade is suitable for every aerospace specification — contact us to confirm availability for your requirement. For general industrial supply, EN1044 conformance is the standard certification. Full material test certificates, conformance certificates and batch traceability records are available on request for all standard grades.

Quick Reference

ApplicationRecommended alloyFluxNotes
General engineering — copper, brass, mild steelAG103 (or AG105/AG107 for cost)GS30Most versatile starting point
Refrigeration copper pipeworkCP102 or CP101None on copper-to-copperGS30 required on brass fittings
HVAC copper pipeworkCP103 or CP102None on copper-to-copperGS30 required on brass fittings
Stainless steelL-AG45SnSiStay-Silv BlackSpecialist flux essential
Nickel alloysL-AG45SnSiStay-Silv BlackNever use copper phosphorus alloys
Tungsten carbide to steelHigh-silver alloyStay-Silv BlackCool slowly — contact us for specification
Aluminium brazingAl12SiAlSi fluxPropane, staged heating
Aluminium soldering and aluminium to dissimilar metalsAlloy 2207Stayclean AluminiumLead-free, low temperature
Plumbing and heating copper pipework (brazed)CP201 or CP202None on copper-to-copperCP103 or CP104 for gas and higher pressure
AerospaceAG103 or L-AG45SnSiGS30 or Stay-Silv BlackFull certification and traceability — contact us
Colour match on polished brassAG104GS30Feed as ring or preform from inside the joint
Production, induction and furnace brazingPreforms or brazing pasteAs alloy, or incorporated in pasteContact us with joint geometry

Still Not Sure? Talk to Our Technical Team.

The alloy selector covers the most common base metal combinations and application requirements, but brazing specifications can be complex — particularly for dissimilar metals, high-integrity applications, automated processes and specialist base metals. If your application is not covered by the selector, or if you want to discuss your specification with a technical expert before ordering, contact our team directly. We are happy to advise without obligation.